hot lamination film - omc-1 Specificaton & Trade Terms
Model | omc-1 |
---|
Place Of Origin | China |
---|
Price Term | EX-Work |
---|
Payment Term | T/T |
---|
hot lamination film
SPECIFICATION & PARAMETER
MATERIAL
Surface layer: BOPP
glue layer: EVA adhesive
SPECIFICATION
Thickness:
Glossy : 18mic (12+6), 20mic (12+8), 22mic (12+10),23mic (15+8),
24mic (12+12) ,25mic (15+10), 27mic (15+12),30mic(18+12)
Matte: 18mic (12+6), 20mic (12+8), 22mic (12+10),23mic (15+8),
24mic (12+12) ,25mic (15+10), 27mic (15+12),30mic(18+12)
Width: 250~1880mm
Length: 100~4000M
Paper core: 25.4mm (1 inch),58mm(2.25inches),76mm(3 inches)
Bonding: less than 2
Process Parameter:
·Equipment for thermal film: dry and wet film laminator
·lamination temperature: 95~105℃
·Roller pressure: 10-20Mpa
·Speed: 8-20 m/min
Directions for using BOPP thermal laminating film:
1. Normal process temperature is 90℃-105℃, roller pressure and temperature vary with different types of paper, ink and machines.
2. When using the film for the first time or do other treatment, try a small volume before mass laminating.
3. Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder.
4. Make sure put the material in a low-temperature, dry place.