tower tray (plate) for zinc smelting - for non-ferrous Specificaton & Trade Terms
Model | for non-ferrous |
---|
Place Of Origin | China |
---|
Price Term | EX-Work |
---|
Payment Term | T/T |
---|
Our tower tray is designed with excellent performance including high strength, good anti-washing resistance of molten zinc, high oxidation resistance and long service life.
Available Size:
990 mm × 457 mm × 165 mm, 1260 mm × 620 mm × 180 mm, 1372 mm × 762 mm × 180 mm, or according to clients’ demands.
Applications:
Designed for zinc vertical retorting.
Typical Technical Parameter:
SiC: > 90%;
Porosity: < 12%;
Volume Density: > 2.7 g/cm3;
Thermal Conductivity: > 15.5 W/ (m•K);
Compressive Strength: > 195 MPa;
Flexural Strength: > 40 MPa;
Working Temperature: 1000-1400 °C.